[en] In this study, the localized corrosion susceptibility of AA2050-T84, AA2198-T851, and AA2024-T3 alloys was compared by immersion in three test solutions, specifically sodium chloride solution (3.5% NaCl), EXCO solution, according to ASTM G34-18, and a solution for intergranular corrosion (IGC) test recommended by ASTM G110-15 and via scanning vibrating electrode technique (SVET). The results showed higher susceptibility of AA2050-T84 alloy to all types of corrosion tested compared to the other studied 2XXX series alloys. Corrosion penetration was deeper in the AA2050-T84 due to its microstructural characteristics as a difference in the micrometric Cu-Rich intermetallic particle distribution on the surface and related to the distribution of the T1 (Al2CuLi) phase.
Research center :
CRIM - Ingénierie des matériaux
Disciplines :
Materials science & engineering
Author, co-author :
Klumpp, Rafael Emil ; Université de Mons - UMONS > Faculté Polytechnique > Service de Science des Matériaux ; Instituto de Pesquisas Energéticas e Nucleares, São Paulo, Brazil
Akbarzadeh, Sajjad ; Université de Mons - UMONS > Faculté Polytechnique > Service de Science des Matériaux
de Sousa Araujo, João Victor; Instituto de Pesquisas Energéticas e Nucleares, São Paulo, Brazil
Gonon, Maurice François ; Université de Mons - UMONS > Faculté Polytechnique > Service de Science des Matériaux
Delaunois, Fabienne ; Université de Mons - UMONS > Faculté Polytechnique > Service de Métallurgie
Costa, Isolda; Instituto de Pesquisas Energéticas e Nucleares, São Paulo, Brazil
Olivier, Marjorie ; Université de Mons - UMONS > Faculté Polytechnique > Service de Science des Matériaux
Language :
English
Title :
Correlating corrosion modes with the microstructure of the 2XXX series alloys: A comparative approach
Publication date :
2024
Journal title :
Surface and Interface Analysis
ISSN :
0142-2421
eISSN :
1096-9918
Publisher :
John Wiley and Sons Ltd
Peer reviewed :
Peer Reviewed verified by ORBi
Development Goals :
9. Industry, innovation and infrastructure
Research unit :
F502 - Science des Matériaux
Research institute :
R400 - Institut de Recherche en Science et Ingénierie des Matériaux
Funders :
Conselho Nacional de Desenvolvimento Científico e Tecnológico Fundação de Amparo à Pesquisa do Estado de São Paulo Fédération Wallonie-Bruxelles
Funding text :
The authors are thankful to CNPq for the financial support for this project (CNPq Proc 406871/2021\u20103) and for the grant awarded to Rafael E. Klumpp (CNPq Proc 200257/2022\u20106) and to the SPW\u2010Economie Emploi Recherche \u2013 Wallonie in the framework of the program OptiSurFam \u2013 Win2Wal (2310020). Additionally, appreciation is extended to the Funda\u00E7\u00E3o de Amparo \u00E0 Pesquisa do Estado de S\u00E3o Paulo (FAPESP), [Process 2019/18388\u20101] Grant of Jo\u00E3o V.S. Araujo, and to the F\u00E9d\u00E9ration Wallonie\u2010Bruxelles (Actions de Recherche Concert\u00E9es ARC SEALCERA \u2013 Grant of Sajjad Akbarzadeh).
Dursun T, Soutis C. Recent developments in advanced aircraft aluminium alloys. Mater des. 2014;56:862-871. doi:10.1016/j.matdes.2013.12.002
Rambabu P., Eswara Prasad N., Kutumbarao V. V. and Wanhill R. J. H., 2017, pp. 29–52.
Araujo JV d S, da Silva RMP, de Viveiros BVG, Klumpp RE, Costa I. Estudo do comportamento eletroquímico de uma liga Al-Cu-Li. Matéria (Rio Janeiro). 2024;29:e20230328. doi:10.1590/1517-7076-rmat-2023-0328
Wanhill R. J. H. and Bray G. H., in Aluminum - Lithium Alloys: Processing, Properties, And Applications, eds. N. E. Prasad, A. Gokhale and R. J. H. Wanhill, Elsevier Inc. 2014, pp. 27–58, doi:10.1016/B978-0-12-401698-9.00002-1.
Milagre M. X., Araujo J. V. de S., Pereira M., Donatus U., Machado C. S. C. and Costa I., in Proceedings of the European Corrosion Congress, 2018.
Donatus U. Corrosion behaviour of friction stir welded aluminium alloys: unpredictability and protection. Res Dev Mater Sci. 2017;2:1-3.
Sousa Araujo JV, Milagre MX, Ferreira RO, et al. Exfoliation and intergranular corrosion resistance of the 2198 Al–cu–Li alloy with different thermomechanical treatments. Mater Corros. 2020;71(12):1957-1970. doi:10.1002/maco.202011839
Birbilis N, Buchheit RG. Electrochemical characteristics of intermetallic phases in aluminum alloys. J Electrochem Soc. 2005;152(4):B140. doi:10.1149/1.1869984
Donatus U, Bodunrin MO, Olayinka A, et al. Advanced Aluminium Composites and Alloys; 2021:159.
Correia AN, Braga DFO, Moreira PMGP, Infante V. Review on dissimilar structures joints failure. Eng Fail Anal. 2021;129:1-14, 105652. doi:10.1016/j.engfailanal.2021.105652
Owolabi GM, Thom M, Ajide O, et al. Fatigue responses of three AA 2000 series aluminum alloys. J Mater Sci Chem Eng. 2019;07(03):32-48. doi:10.4236/msce.2019.73003
Buchheit RG, Moran JP, Stoner GE. Localized corrosion behavior of alloy 2090—the role of microstructural heterogeneity, corrosion. 1990;46(8):610-617. doi:10.5006/1.3585156
Buchheit RG, Moran JP, Stoner GE. Electrochemical behavior of the T 1 (Al 2 CuLi) intermetallic compound and its role in localized corrosion. Corros Sci. 1994;50(2):120-130. doi:10.5006/1.3293500
Ma Y, Zhou X, Huang W, et al. Crystallographic defects induced localised corrosion in AA2099-T8 aluminium alloy. Corros Eng Sci Technol. 2015;50(6):420-424. doi:10.1179/1743278214Y.0000000237
Zhang X, Zhou X, Hashimoto T, et al. The influence of grain structure on the corrosion behaviour of 2A97-T3 Al-Cu-Li alloy. Corros Sci. 2017;116:14-21. doi:10.1016/j.corsci.2016.12.005
Huang J, Li J, Liu D, et al. Correlation of intergranular corrosion behaviour with microstructure in Al-Cu-Li alloy. Corros Sci. 2018;139:215-226. doi:10.1016/j.corsci.2018.05.011
Milagre MX, Donatus U, Mogili NV, et al. Galvanic and asymmetry effects on the local electrochemical behavior of the 2098-T351 alloy welded by friction stir welding. J Mater Sci Technol. 2020;45:162-175. doi:10.1016/j.jmst.2019.11.016
Donatus U, Ferreira RO, Mogili NVV, de Viveiros BVG, Milagre MX, Costa I. Corrosion and anodizing behaviour of friction stir weldment of AA2198-T851 Al-Cu-Li alloy. Mater Chem Phys. 2018;219:493-511. doi:10.1016/j.matchemphys.2018.08.053
Donatus U, de Sousa Araujo JV, de Souza Carvalho Machado C, Vardhan Mogili NV, Antunes RA, Costa I. The effect of manufacturing process induced near-surface deformed layer on the corrosion behaviour of AA2198-T851 Al–Cu–Li alloy. Corros Eng Sci Technol. 2018;2782(3):1-11. doi:10.1080/1478422X.2018.1558932
Viveiros BVGD, Donatus U, de Alencar MC, Berbel LO, Costa I. Comparing the corrosion behaviour of AA2050 and AA7050 aluminium alloys by scanning vibrating electrode and scanning ion-selective electrode techniques. Corros Eng Sci Technol. 2022;57(1):85-96. doi:10.1080/1478422X.2021.1992132
Zhang S, Zeng W, Yang W, Shi C, Wang H. Ageing response of a Al-Cu-Li 2198 alloy. Mater des. 2014;63:368-374.
Buchheit RG, Grant RP, Hiava PF, Mckenzie B, Zender G. Local dissolution phenomena associated with S phase (AI2CuMg) particles in aluminum alloy 2024-T3. J Electrochem Soc. 1997;144(8):2621-2628. doi:10.1149/1.1837874
Donatus U, de Viveiros BVG, de Alencar MC, et al. Correlation between corrosion resistance, anodic hydrogen evolution and microhardness in friction stir weldment of AA2198 alloy. Mater Charact. 2018;144:99-112. doi:10.1016/j.matchar.2018.07.004
de Souza Carvalho Machado C, da Silva RMP, de Sousa Araujo JV, et al. Influence of chloride ions concentration on the development of severe localised corrosion and its effects on the electrochemical response of the 2198-T8 alloy. Corros Eng Sci Technol. 2021;56(4):341-350. doi:10.1080/1478422X.2020.1862390
da Silva RMP, Milagre MX, de Oliveira LA, Donatus U, Antunes RA, Costa I. The local electrochemical behavior of the AA2098-T351 and surface preparation effects investigated by scanning electrochemical microscopy. Surf Interface Anal. 2019;51(10):982-992. doi:10.1002/sia.6682
Alexopoulos ND, Proiou A, Dietzel W, et al. Mechanical properties degradation of (Al-Cu-Li) 2198 alloy due to corrosion exposure. Procedia Struct Integr. 2016;2:597-603. doi:10.1016/j.prostr.2016.06.077
Queiroz FM, Magnani M, Costa I, de Melo HG. Investigation of the corrosion behaviour of AA 2024-T3 in low concentrated chloride media. Corros Sci. 2008;50(9):2646-2657. doi:10.1016/j.corsci.2008.06.041
de Abreu CP, Costa I, de Melo HG, Pébère N, Tribollet B, Vivier V. Multiscale electrochemical study of welded Al alloys joined by friction stir welding. J Electrochem Soc. 2017;164(13):C735-C746. doi:10.1149/2.0391713jes
Bugarin AFS, Queiroz FM, Terada M, De Melo HG, Costa I. Localized corrosion resistance of dissimilar aluminum alloys joined by friction stir welding (FSW). Key Eng Mater. 2016;710:41-46. doi:10.4028/www.scientific.net/KEM.710.41
Bousquet E, Poulon-Quintin A, Puiggali M, Devos O, Touzet M. Relationship between microstructure, microhardness and corrosion sensitivity of an AA 2024-T3 friction stir welded joint. Corros Sci. 2011;53(9):3026-3034. doi:10.1016/j.corsci.2011.05.049
Palomino LEM. Caracterização microestrutural e eletroquímica de revestimentos ambientalmente amigaveis aplicados sobre a liga de AL2024-T3 - [Tese]. 2007;265.
Alam MP, Sinha AN. Fabrication of third generation Al–Li alloy by friction stir welding: a review. Sadhana - Acad Proc Eng Sci. 2019;44(6):1-13, 153. doi:10.1007/s12046-019-1139-4
Machado C d SC, Donatus U, Giorjão RAR, et al. Proceedings of the European Corrosion Congress; 2018:26.
Milagre MX, Mogili NV, Donatus U, et al. On the microstructure characterization of the AA2098-T351 alloy welded by FSW. Mater Charact. 2018;140:233-246. doi:10.1016/j.matchar.2018.04.015
Lu D, Li J, Ning H, et al. Effects of microstructure on tensile properties of AA2050-T84 Al − Li alloy. Trans Nonferrous Met Soc Chin. 2021;31(5):1189-1204. doi:10.1016/S1003-6326(21)65571-1
Jagadeesh C. Effect of multi-directional forging on the evolution of microstructural and mechanical properties of lightweight Al-Cu-Li alloy AA2050. J Mater Eng Perform. 2023;1–15(24):11118-11132. doi:10.1007/s11665-023-07922-5
Proton V, Alexis J, Andrieu E, et al. The influence of artificial ageing on the corrosion behaviour of a 2050 aluminium-copper-lithium alloy. Corros Sci. 2014;80:494-502. doi:10.1016/j.corsci.2013.11.060
Donatus U, Terada M, Ospina CR, Queiroz FM, Bugarin AFS, Costa I. On the AA2198-T851 alloy microstructure and its correlation with localized corrosion behaviour. Corros Sci. 2018;131:300-309. doi:10.1016/j.corsci.2017.12.001
Donatus U, Klumpp RE, Vardan Mogili NV, Antunes RA, Milagre MX, Costa I. The effect of surface pretreatment on the corrosion behaviour of silanated AA2198-T851 Al-Cu-Li alloy. Surf Interface Anal. 2019;51(2):275-289. doi:10.1002/sia.6584
Donatus U, da Silva RMP, Araujo JV d S, et al. Macro and microgalvanic interactions in friction stir weldment of AA2198-T851 alloy. J Mater Res Technol. 2019;8(6):6209-6222. doi:10.1016/j.jmrt.2019.10.015
Steuwer A, Dumont M, Altenkirch J, et al. A combined approach to microstructure mapping of an Al-Li AA2199 friction stir weld. Acta Mater. 2011;59(8):3002-3011. doi:10.1016/j.actamat.2011.01.040
Proton V, Alexis J, Andrieu E, Delfosse J, Lafont M-C, Blanc C. Characterisation and understanding of the corrosion behaviour of the nugget in a 2050 aluminium alloy friction stir welding joint. Corros Sci. 2013;73:130-142. doi:10.1016/j.corsci.2013.04.001
Machado CSC, Klumpp RE, Ayusso VH, et al. Effect of surface treatments on the localized corrosion resistance of the AA2198-T8 aluminum lithium alloy welded by FSW process. Surf Interface Anal. 2019;51(12):1231-1239. doi:10.1002/sia.6622
Klumpp RE, Donatus U, Araujo JVS, Redígolo MM, Machado C d SC, Costa I. The effect of acid pickling on the corrosion behavior of a cerium conversion-coated AA2198-T851 Al-Cu-Li alloy. J Mater Eng Perform. 2020;29(1):167-174. doi:10.1007/s11665-019-04551-9